This process does not contain sodium cyanide (potassium) and silver cyanide, does not contain phosphorus, wastewater treatment is simple, in line with environmental requirements. 2. This process is compatible with cyanide silver plating solution and can be directly transferred to the cylinder on the basis of cyanide silver plating solution. 3. Depending on the needs, with different additives can be obtained thin silver or thick silver and other decorative or functional coatings.

Still deciding? Get samples first,  Contact US !

View similar products

Tag list

  • Product Description
  • Solution composition and operating conditions

     

     Scope
    Silver nitrateThin silver: 3-5g/L
    Thick silver: 25-30g/l
    DZ-370 environmental protection sodium salt500-900 ml/l
    Potassium hydroxide10g/l
    Temperature20-30 ℃
    current density0.3-1 amp/square decimeter
    anodeSterling silver plate or 316 stainless steel mesh
    Anode to cathode area ratio≧ 2:1
    StirringAir agitation or cathode movement
    Anode sleeve materialPolyester, nylon

     

     

DZ-370 Environmentally friendly silver plating process

This process does not contain sodium cyanide (potassium) and silver cyanide, does not contain phosphorus, wastewater treatment is simple, in line with environmental requirements. 2. This process is compatible with cyanide silver plating solution and can be directly transferred to the cylinder on the basis of cyanide silver plating solution. 3. Depending on the needs, with different additives can be obtained thin silver or thick silver and other decorative or functional coatings.

Still deciding? Get samples first,  Contact US !

Products Category

Tag list

Inquire Now

Note: Please leave your email address, our professionals will contact you as soon as possible!