Solution composition and operating conditions
DZ-2805 30-120g/l Hydrochloric acid 0-20 ml/l Time 2-10 minutes Temperature 30-50 ℃
DZ-2805 Plastic electroplating degumming process
1. Effectively reduce the rate of defective products at the contact point of the hanging tool.
2. Wide process range and easy operation.
3. A uniform electroless nickel coating can also be obtained by appropriately reducing the concentration of the palladium activator.
Still deciding? Get samples first, Contact US !
Products Category
Tag list
Inquire Now
Note: Please leave your email address, our professionals will contact you as soon as possible!