• DZ-2804 Plastic electroplating palladium activation process
DZ-2804 Plastic electroplating palladium activation process
+

DZ-2804 Plastic electroplating palladium activation process

1. Mixed with hydrochloric acid, dedicated to plastic electroplating, the catalysis of the Pd-Sn system before electroless nickel plating can obtain a uniform electroless coating. 2.DZ-2804 activator is stable and has long service life.

Still deciding? Get samples first,  Contact US !

View similar products

Tag list

  • Product Description
  • Solution composition and operating conditions

     

    Pure water710-750 ml/l
    37% hydrochloric acid (analytically pure)250-280 ml/l
    DZ-2804 activator3-6 ml/l
    Time2-6 minutes
    Temperature21-32 ℃

     

     

DZ-2804 Plastic electroplating palladium activation process

1. Mixed with hydrochloric acid, dedicated to plastic electroplating, the catalysis of the Pd-Sn system before electroless nickel plating can obtain a uniform electroless coating. 2.DZ-2804 activator is stable and has long service life.

Still deciding? Get samples first,  Contact US !

Products Category

Tag list

Inquire Now

Note: Please leave your email address, our professionals will contact you as soon as possible!