Solution composition and operating conditions
Chromic Anhydride 360-400g/l sulfuric acid 360-400g/l DZ-2802 2-8 ml/l Time 6-10 minutes Temperature 55-62 ℃
DZ-2802 Plastic electroplating roughening process
1. Make the surface of the workpiece produce a uniform rough surface.
2. Improve the bonding force between the workpiece and the coating.
3. Improve the wettability and foaming of the roughening liquid, inhibit the escape of acid mist, and reduce the loss of roughening liquid.
Still deciding? Get samples first, Contact US !
Products Category
Tag list
Inquire Now
Note: Please leave your email address, our professionals will contact you as soon as possible!