• HKS-301E Galvanizing Sealer Process
HKS-301E Galvanizing Sealer Process
+

HKS-301E Galvanizing Sealer Process

1. A water-soluble galvanized sealing agent, suitable for all galvanized passivation after sealing, suitable for hanging plating and barrel plating parts; 2. The sealing layer of HKS-301E galvanizing sealant is heat-resistant at 120 ℃ for 24 hours. It has good corrosion resistance, and the neutral salt spray can reach the standard for 100-200 hours.

Still deciding? Get samples first,  Contact US !

View similar products

Tag list

  • Product Description
  • Solution composition and operating conditions

     

    Sealer for HKS-301E galvanizing10-30%
    Impregnation temperatureRoom temperature -40 ℃ (heating by indirect heating)
    Impregnation time10-60 seconds
    Exposed time1*-3min
    pH9.0-10.0
    Drying temperature/drying time70-120 ℃ 10-30min
    Solid content1.8-5.0%

     

     

HKS-301E Galvanizing Sealer Process

1. A water-soluble galvanized sealing agent, suitable for all galvanized passivation after sealing, suitable for hanging plating and barrel plating parts; 2. The sealing layer of HKS-301E galvanizing sealant is heat-resistant at 120 ℃ for 24 hours. It has good corrosion resistance, and the neutral salt spray can reach the standard for 100-200 hours.