DZ-60S Pearl Nickel Plating Process
1. The coating structure is meticulous, the hardness is high, the wear resistance is good, and it is not easy to be scratched.
2. The coating has strong corrosion resistance and is not easy to be corroded or leave traces.
3. The sand speed is fast, the decomposition product is less, and the plating solution is easy to control.
4. Users can choose K2, K4, K6 according to the requirements of the product to achieve the required thickness.
5. This product is a long-term process with a long processing cycle.
Still deciding? Get samples first, Contact US !
View similar products
Tag list
- Product Description
-
Solution composition and operating conditions
Nickel sulfate 380-420g/l Nickel chloride 35-45g/l boric acid 30-40g/l DZ-60K pearl nickel cylinder opener 15-20 ml/l DZ-60H pearl nickel walking agent 3-8 ml/l DZ-60T pearl nickel regulator 2-4 ml/L (add as needed) DZ-60S(K2/K4/K6) Pearl Nickel Sand 0.3-0.8 ml/l pH 4.2-4.8 Temperature 50-60 ℃ cathode current density 3-8 amps/square decimeter plating time 2-5 minutes
DZ-60S Pearl Nickel Plating Process
1. The coating structure is meticulous, the hardness is high, the wear resistance is good, and it is not easy to be scratched.
2. The coating has strong corrosion resistance and is not easy to be corroded or leave traces.
3. The sand speed is fast, the decomposition product is less, and the plating solution is easy to control.
4. Users can choose K2, K4, K6 according to the requirements of the product to achieve the required thickness.
5. This product is a long-term process with a long processing cycle.